Productgegevens
Betaling en verzendvoorwaarden
Chemical Resistance: |
Excellent |
Breakdown Voltage: |
20-25 KV/mm |
Melting Point: |
1900°C |
Insulation Resistance: |
1012-1014 Ω.cm |
Dimension: |
128*17*4mm |
Dielectric Constant: |
9.2-9.6 |
Compressive Strength: |
3,000 MPa |
Lead Time: |
30days |
Port: |
Shanghai |
Colour: |
dark grey |
Feature: |
high stength resistance |
Processing Service: |
Bending, Welding, Cutting, Moulding |
Origin: |
China |
Relative Density: |
99% |
Type: |
Ceramic Parts |
Chemical Resistance: |
Excellent |
Breakdown Voltage: |
20-25 KV/mm |
Melting Point: |
1900°C |
Insulation Resistance: |
1012-1014 Ω.cm |
Dimension: |
128*17*4mm |
Dielectric Constant: |
9.2-9.6 |
Compressive Strength: |
3,000 MPa |
Lead Time: |
30days |
Port: |
Shanghai |
Colour: |
dark grey |
Feature: |
high stength resistance |
Processing Service: |
Bending, Welding, Cutting, Moulding |
Origin: |
China |
Relative Density: |
99% |
Type: |
Ceramic Parts |
Siliciumnitride ((Si3N4)) overtreft veel andere keramische materialen in thermische schokbestendigheid.het is ideaal voor gebruik in onderdelen voor automobielmotoren en gasturbines, met inbegrip van turbocompressorrotorenHet is de bedoeling dat deze technologie in een breed scala van gebieden verder wordt toegepast.